Abstract
Objective: Zirconium oxide has gained the spotlight during the recent years as a high strength ceramic material. However, despite its mechanical superiorities, it forms a weak bond with different synthetic substrates and tissues due to its neutral nature and resistance against chemical agents. Therefore, it is important to improve the bonding technique in order to prevent microleakage and increase retention and fracture resistance of the restoration.
Literature Review: Since the discovery of zirconium oxide, several surface treatment methods have been evaluated to increase its bond strength to resin cement such as surface grinding with micro- abrasion, burs or abrasive papers, tribochemical silica coating, silicoating, glass micropearls, glaze- on technique, selective infiltration etching, hot etching and use of phosphate ester monomers. The mentioned techniques and related articles are reviewed and discussed in the present study.
Conclusion: Despite extensive studies, no consensus has been reached about a specific treatment as the standard protocol for improving the bond strength of zirconia restorations.- Bond strength
- High strength ceramics
- Neutral nature
- Resin cement
- Surface treatment
- Zirconium oxide
How to Cite
References
Thompson JY, Stoner BR, Piascik JR, Smith R. Adhesion/cementation to zirconia and other non- silicate ceramics: Where are we now? Dent Mater 2011; 27:71-82.
Denry I, Kelly JR. State of the art of zirconia for dental applications. Dent Mater 2008; 24: 299- 307.
Mehta D, Shetty R. Bonding to zirconia: elucidating the confusion. International Dentistry SA 2010; 12:46-52.
Heuer AH, Lange FF, Swain MV, Evans AG. Transformation toughening: an overview. J Am Ceram Soc 1986; 69: i- iv.
Sakaguchi RL, Powers JM. Craig’s restorative dental materials. 13th Ed. Philadelphia: Elsivier
; Chap 11:253-275.
Chevalier J, Olagnon C, Fantozzi G. Crack propagation and fatigue in zirconia-based composites. Compos Part A Appl Sci Manuf 1999; 30: 525-530.
Chevalier J. What future for zirconia as a biomaterial? Biomaterials 2006; 27: 535-543.
Kern M, Wegner SM. Bonding to zirconia ceramic: Adhesion methods and their durability. Dent Mater 1998; 14: 64-71.
Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003; 89: 268-274.
Blatz MB, Sadan A, Arch GH, Lang BR. In vitro evaluation of long-term bonding of Procera All Ceram alumina restorations with modified resin luting agent. J Prosthet Dent 2003; 89: 381-387.
Blatz MB, Chiche G, Holst S, Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 2007; 38: 745-53.
Piascik JR, Wolter SD, Stoner BR. Development of a novel surface modification for improved bonding to zirconia. Dent Mater 2011; 27: e99-105.
Amaral R, Ozcan M, Bottino MA, Valandro LF. Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning. Dent Mater 2006; 22: 283-290.
Bottino MA, Valandro LF, Scotti R, Buso L. Effect of surface treatments on the resin bond to zirconium-based ceramic: Int J Prosthodont 2005; 18: 60-65.
Blatz MB, Sadan A, Kern M. Bonding to silica-based ceramics: clinical and laboratory guidelines. Quintessence Dent Technol 2002; 25: 54-62.
Lohbauer U, Zipperle M, Rischka K, Petschelt A, Muller FA. Hydroxilation of dental zirconia surfaces: Characterization and bonding potential. J Biomed Mater ResBomater2008; 87:461–467.
Wegner SM, Kern M. Long term resin bond strength to zirconia ceramic. J Adhes Dent 2000 Summer; 2: 139-47.
Wegner SM, Gerdes W, Kern M. Effect of different artificial aging conditions on ceramic- composite bond strength. Int J Prosthodont 2002; 15: 267-72.
Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000; 13: 131-5.
Atsu SS, Lilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006; 95: 430-6.
Piwowarczyk A, Lauer HC, Sorensen JA. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 2005; 30: 382-8.
Harris AF, Beevers A. The effect of grit-blasting on surface properties for adhesion. Int J Adhes 1999; 19: 445-452.
Holmberg K, Ronkainen H, Mathew A. Tribology of thin coatings. Ceram Int 2000; 26: 787-95.
Shigeyasu A, Akira S. Fractal analysis of surface roughened by grit blasting. J Adhes Sci Technol 2000; 14: 27-41.
Zhang Y, Lawn BR, Rekow ED, Thompson VP. Effect of sandblasting on the long-term performance of dental ceramics. J Biomed Mater Res B Appl Biomater 2004; 71B: 381-6.
Sato H, Yamada K, Pezzotti G, Nowa M, Ban S. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater 2008; 27: 408-14.
Curtis AR, Wright AJ, Fleming GJP. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent 2006; 34: 195-206.
Cavalcanti AN, Foxton RM, Watson TF, Oliveira MT, Giannini M, Marchi GM. Bond strength of resin cements to a zirconia ceramic with different surface treatments. Oper Dent 2009; 34: 268-78.
Kern M. Resin bonding to oxide ceramics for dental restorations.J Adhes Sci Technol 2009; 23: 1097-111.
Xible AA, de Jesus Tavarez RR, Araujocdos R, Bonachela WC. Effect of silica coating and silanization on flexural and composite-resin bond strength of zirconia posts: An in vitro study. J Prosthet Dent 2006; 95: 224-9.
Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of YTZP zirconia ceramic. Dent Mater 1999; 15: 426-433.
Hallmann L, Ulmer P, Reusser EH, Hämmerle C. Surface characterization of dental YTZP ceramic after air abrasion treatment. J Dent 2012; 40: 723-35.
Lawn BR, Deng Y, Lioyd IK, Janal MN, Rekow ED, Thompson VP. Materials design of ceramic- based layer structures for crowns. J Dent Res 2002; 81: 433-438.
Guess PC, Zhang Y, Kim JW, Rekow ED, Thompson VP. Damage and reliability of Y-TZP after cementation surface treatment. J Dent Res. 2010; 89(6): 592-6.
Magne P, Paranhos MP, Burnett LH. New zirconia primer improves bond strength of resin-based cements. Dent Mater 2010; 26: 345-352.
Monaco C, Cardelli P, Scotti R, Valandro LF. Pilot evaluation of four experimental conditioning treatments to improve the bond strength between resin cement and Y-TZP ceramic. J Prosthodont 2011; 20: 97-100.
Moon JE, Kim SH, Lee JB, Ha SR, Choi YS. The effect of preparation order on the crystal structure of yttria-stabilized tetragonal zirconia polycrystal and the shear bond strength of dental resin cements. Dent Mater 2011; 27: 651-663.
Stangel I, Nathanon D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res 1987; 66: 1460-1465.
Matinlinna JP, Lassila LV, Vallittu PK.The effect of three silane coupling agents and their blends with a cross-linker silane on bonding a bis-GMA resin to silicatized titanium (a novel silane system). J Dent 2006; 34: 740-746.
Matinlinna JP, Lassila LV, Kangasniemi I, Vallittu PK. Isocyanato- and methacryloxysilanes promote bis-GMA adhesion to titanium. J Dent Res 2005; 84: 360-364.
Matinlinna JP, Heikkinen T, Ozcan M, Lassila LVJ, Vallittu PK.Evaluation of resin adhesion to zirconia ceramic using some organosilanes Dent Mater 2006; 22: 824-831.
Heikkinen TT, Lassila LV, Matinlinna JP, Vallitu PK. Effect of operating air pressure on tribochemical silica-coating. Acta Odontol Scand 2007; 65: 241-248.
Takeuchi K, Fujishima A, Manabe A, Kuiyama S, Hotta Y. Combination treatment of tribochemical treatment and phosphoric acid ester monomer of zirconia ceramics enhances the bonding durability of resin-based luting agents. Dent Mater J 2010; 29: 316-323.
Derand T, Molin M, Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 2005; 21: 1158-1162.
Kitayama S, Nikaido T, Maroka R, Zhu L, Ikeda M, Watanabe A, et al. Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics. Dent Mater J 2009; 28: 446-453.
Jevnikar P, Krnel K, Kocjan A, Funduk N, Kosmac T. The effect of nano-structured alumina coating on resin-bond strength to zirconia ceramics. Dent Mater 2010; 26: 688-696.
Ntala P, Chen X, Niggli I, Cattell M. Development and testing of multi-phase glaze for adhesive bonding to zirconia substrates. J Dent 2010; 38: 773-781.
Valentino TA, Borges GA, Borges LH, Platt JA, Correr-Sobrinho L. Influence of glazed zirconia on dual-cure luting agent bond strength. Oper Dent. 2012; 37: 181-187.
Everson P, Addison O, Palin WM, Burke F. Improved bonding of zirconia substructures to resin using a “glaze-on” technique. J Dent 2012; 40: 347-351.
Cura C, Ozcan M, Isik G, Saracoglu A. Comparison of alternative adhesive cementation concepts for zirconia ceramic: glaze layer vs zirconia primer. J Adhes Dent 2011; 14: 75-82.
Musil R, Tiller HJ. The adhesion of dental resin to metal surfaces. The Kulzer silicoater technique. Gmb: Wehrbeim Kulzer and Co. 1984: 9-53.
Mazurat RD, Pesun S. Resin-metal bonding systems: a review of the silicoating and kevloc systems. J Can Dent Assoc 1998; 64: 503-507.
Janda R, Roulet JF, Wulf M, Tiller HJ. A new adhesive technology for all-ceramics. Dent Mater 2003; 19: 567-573.
Peutzfeldt A, Asmussen E. Silicoating. Evaluation of a new method of bonding composite resin to metal. Scand J Dent Res 1988; 96: 171-176.
Hansson O, Moberg LE. Evaluation of three silicoating methods for resin-bonded prosthesis. Scand J Dent Res1993; 101: 243-251.
Hummel SK, Pace LL, Marker VA. A comparison of two silicoating techniques. J Prosthodont 1994; 3:108-113.
Kobrin B, Chinn J, Ashurst RW. Durable anti stiction coatings by molecular vapor deposition (MVD). NSTI Nanotech 2005; 2: 247-350.
Piascik JR, ,SwiftEJ,Thompson JY, Grego S, Stoner BR. Surface modification for enhanced silanation of high zirconia ceramics. Dent Mater 2009; 25: 1116-1121.
Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration-etching technique for a strong and durable bond of resin cement to zirconia-based materials. J Prosthet Dent 2007; 98: 379-388.
Aboushelib MN, Matinlinna JP, Salameh Z, Ounsi H. Innovations in bonding to zirconia-based materials: part I. Dent Mater. 2008; 24: 1268-1272.
Aboushelib MN, Feilzer AJ, Kleverlaan CJ. Bonding to zirconia using a new surface treatment. J Prosthodont 2010; 19: 340-346.
Casucci A, Osorio E, Osorio R, Monticelli F, Toledano M, Mazzitelli C, et al. Influence of different surface treatments on surface zirconia frameworks. J Dent 2009; 37: 891-897.
Casucci A, Monticelli F, Goracci C, Mazzitelli C, Cantoro A, Papacchini F, Ferarin M. Effect of surface pre-treatments on the zirconia ceramic-resin cement microtensile bond strength. Dent Mater J 2011; 27: 1024-1030.
Javid AH, Hassani AH, Golshan G. Selective removal of heavy metals from ferric chloride caused by etching processes by using sulfide precipitation. J EnvSci Tech 2004; 20.
Kumbuloglu O, Lassila LV, User A, Vallittu PK. Bonding of resin composite luting cements to zirconium oxide by two air-particle abrasion methods. Oper Dent 2006; 31: 248-255.
Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007; 23: 45-50.
Kern M, Thompson VP. Bonding to a glass infiltrated alumina ceramics: adhesive methods and their durability. J Prosthet Dent 1995; 73: 240-249.
Denry IL. Recent advances in ceramic for dentistry. Crit Rev Oral Biol Med 1996; 7:134-143.
Blatz MB, Richter C, Sadan A, Chiche GJ. Critical appraisal. Resin bond to dental ceramics part II: high-strength ceramics. J Esthet Rest tor Dent 2004; 16: 324-328.
Luthy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006; 22: 195-200.
Lorenzoni F, Leme V, Santos L, de Oliveira P, Martins L, Bonfante G. Evaluation of chemical Teatment on Zirconia Surface with Two primer gents and an lkaline Solution on Bond Strength. Oper Dent 2012; 37: 625-633.
Usumez A, Hamdemirci N, Koroglu BY, Simse I, Parlar O, Sari T. Bond strength of resin cement to zirconia ceramic with different surface treatments. Lasers Med Sci 2013; 28: 259-266.
Paranhos MP, Burnett LH, Magne P. Effect of Nd:YAG laser and CO2 laser treatment on the resin bond strength to zirconia ceramic. Quintessence Int 2011; 42: 79-89.
Akyil MS, Uzun IH, Bayindir F. Bond strength of resin cement to yttrium-stabilized tetragonal zirconia ceramic treated with air abrasion, silica coating and laser irradiation. Photomed Laser Surg 2010; 28: 801-808.
Senyilmaz DP, Palin WM, Shortall AC, Burke FJ. Theeffect of surface preparation and luting agent on bondstrength to a zirconium-based ceramic. Oper Dent 2007; 32: 623-630.